Corrosion Resistant Alloy
Hastelloy B (CHINA:NS321)
Hastelloy B-2 (CHINA:NS322)
Hastelloy B-3 (CHINA: )
Hastelloy C (CHINA:NS333)
Hastelloy C-4 (CHINA: )
Hastelloy C-22 (CHINA:)
Hastelloy C-276 (CHINA:NS334)
Hastelloy C-2000 (CHINA:)
Hastelloy X (CHINA:GH3536)
Incoloy 800 (CHINA:NS111)
Incoloy 800H (CHINA:NS112)
Incoloy 825 (CHINA:NS142)
Inconel 600 (CHINA:NS312)
Inconel 625 (CHINA:NS336)
Inconel 718 (CHINA:GH4169)
UNS N04400、Monel 400
UNS N05500、Monel K500
Alloy 20 (CHINA:NS143)
Inconel 601 (CHINA:NS313)
Inconel 690 (CHINA:NS315)
Superalloys
GH1035 (RUSSIA:XH38BT)
GH2132 (US: UNSS66286)
GH3536 (US: Hastelloy X)
GH145 (US: Inconel X-750)
K406 (US: GMR-235D)
K418 (US: INCO713C)
K213 (US:ЭИ787Л)
K417 (US:IN100)
Stainless Steels
904L(CHINA:00Cr20Ni25Mo4.5Cu)
SAF 2205CHINA:00Cr22Ni5Mo3N)
SAF 2207CHINA:00Cr25Ni7Mo4N)
2RE69 (CHINA:00Cr25Ni22M02N)
Alloy 253MA (GERMANY:1.4835)
430 (CHINA:1Cr17Ni2)
310S(CHINA:0Cr25Ni20)
AISI616 (CHINA:2Cr12NiMoWV)
304(CHINA:0Cr18Ni9)
316(CHINA:0Cr17Ni12Mo2)
305 (CHINA:1Cr18Ni12Mo2N)
316Lmod (CHINA:00Cr17Ni14Mo2N)
S21800 (Nitronic 60/218alloy)
254SMO(CHINA:00Cr20Ni18Mo6CuN)
17-4PH(630)(CHINA:0Cr17Ni4Mo4Nb)
17-7PH(631)(CHINA:0Cr17Ni7Al)
304N2 (US:UNS S30452)
AL-6XN (CHINA:00Cr20Ni24Mo7N)
Nitronic 40、UNS20904
Nitronic 50、UNS20910
Nimonic 75、UNS N06075
Nimonic 80A、UNS N07080
Nimonic 90、UNS N07090
Nimonic 263、UNS N07263
HOME ABOUT US PRODUCTS NEWS CONTACT US 中文

Stainless Steels

904L(CHINA:00Cr20Ni25Mo4.5Cu)
 

Physical Properties:
Density:8.0g/cm3                                        Melting Point:1398℃
Modulus of Elasticity:167-188GPa         Thermal Conductivity:12.9λ/(W(m•℃)
Hardness:HRC70-90                      Electrical Resistivity( 20 - 100°C):15x10-6K-1
Approx Service Temperature:-200 to +300℃
Main Characteristics:Austenitic high nickel and low carbon Stainless Steel; good pitting corrosion resistance and stress corrosion cracking resistance.
Applications:Applied in acetic acid making column distiller, ethyne making decontaminating column, sulphuric acid transport pipeline and storage tank etc
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Mo Fe Cu Mn Si P S others


0.02

19.0
-
23.0

23.0
-
28.0

4.0
-
5.0

rem

1.0
-
2.0


2.0


1.0


0.045


0.035

-

 

SAF 2205、UNS S31803(CHINA:00Cr22Ni5Mo3N)
 

Physical Properties:
Density: 7.85g/cm3                                       Melting Point: ℃
Modulus of Elasticity:160-200GPa            Thermal Conductivity:16λ/(W(m•℃)
Hardness:HB260                      Electrical Resistivity( 20 - 100°C): 13.0x10-6K-1
Approx Service Temperature:-200 to +300°C
Main Characteristics: Excellent corrosion resistance and mechanical properties.
Applications:Used in petroleum, fertilizer, paper making and chemical industrie-s and heat exchanger and sprinkler valve in hot aquafortis or sea water media
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Mo Fe N Mn Si P S others


0.03

21.0
-
23.0

4.50
-
6.50

2.50
-
3.50

rem

0.08
-
0.20


2.0


1.0


0.03


0.02

-

 

SAF 2507、UNS S32750(CHINA:00Cr25Ni7Mo4N)
 

Physical Properties:
Density:7.8g/cm3                                      Melting Point: ℃
Modulus of Elasticity:29 psi x 10 6         Thermal Conductivity:8.7Btu/h ft °F
Hardness:HRC32                      Electrical Resistivity( 20 - 100): 7.2x10-6/°F
Approx Service Temperature:-200 to +300°C
Main Characteristics: Excellent corrosion resistance and mechanical properties.
Applications:Used in petroleum, fertilizer, paper making and chemical industri-es and heat exchanger and sprinkler valve in hot aquafortis or sea water media
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Mo Fe N Mn Si P S Cu


0.03

24.0
-
26.0

6.0
-
8.0

3.0
-
5.0

rem

0.24
-
0.32


1.20


0.80


0.035


0.020


0.50

 

2RE69、UNS S31050(CHINA:00Cr25Ni22M02N)
 

Physical Properties:
Density: 7.9g/cm3                                       Melting Point: ℃
Modulus of Elasticity:158-195 GPa         Thermal Conductivity:13W/m °C
Hardness:Rockwell B95          Electrical Resistivity( 20 - 100): 15.5 x10-6
Approx Service Temperature:-200 to +300°C
Main Characteristics:Excellent corrosion resistance and welding properties
Applications:Mainly used in chemical, petroleum and urea equipments.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Mo Fe N Mn Si P S others


0.03

24.0
-
26.0

20.5
-
23.5

1.6
-
2.0

rem

0.09
-
0.16


2.0


0.4


0.020


0.015

-

 

 Copyright © Nanjing Interan Super Alloy CO.,LTD
 Contact: 任卫平   张利利   David
 TEL: 86-025-84170556/84190181/84170331 FAX: 86-025-84170556
 Cellphone Number: 13805152311 / 13770667940
 Zip Code: 211135
 Add:Jiannan Industry Park Cangbomen Jiangning District Nanjing CHINA
 E-mail:Inconel718@163.com / superalloycn@gmail.com
 Web: http://www.superalloy.net.cn

Internet Content Provider Licence of Ministry of Telecom&information Industry PRC Serial No.Jiangsu 0603728