Miss Zhang
 International Dept David Zhu
 
PRODUCTS
Corrosion Resistant Alloy
Hastelloy B (CHINA:NS321)
Hastelloy B-2 (CHINA:NS322)
Hastelloy B-3 (CHINA: )
Hastelloy C (CHINA:NS333)
Hastelloy C-4 (CHINA: )
Hastelloy C-22 (CHINA:)
Hastelloy C-276 (CHINA:NS334)
Hastelloy C-2000 (CHINA:)
Hastelloy X (CHINA:GH3536)
Incoloy 800 (CHINA:NS111)
Incoloy 800H (CHINA:NS112)
Incoloy 825 (CHINA:NS142)
Inconel 600 (CHINA:NS312)
Inconel 625 (CHINA:NS336)
Inconel 718 (CHINA:GH4169)
UNS N04400、Monel 400
UNS N05500、Monel K500
Alloy 20 (CHINA:NS143)
Inconel 601 (CHINA:NS313)
Inconel 690 (CHINA:NS315)
Superalloys
GH1035 (RUSSIA:XH38BT)
GH2132 (US: UNSS66286)
GH3536 (US: Hastelloy X)
GH145 (US: Inconel X-750)
K406 (US: GMR-235D)
K418 (US: INCO713C)
K213 (US:ЭИ787Л)
K417 (US:IN100)
Stainless Steels
904L(CHINA:00Cr20Ni25Mo4.5Cu)
SAF 2205CHINA:00Cr22Ni5Mo3N)
SAF 2207CHINA:00Cr25Ni7Mo4N)
2RE69 (CHINA:00Cr25Ni22M02N)
Alloy 253MA (GERMANY:1.4835)
430 (CHINA:1Cr17Ni2)
310S(CHINA:0Cr25Ni20)
AISI616 (CHINA:2Cr12NiMoWV)
304(CHINA:0Cr18Ni9)
316(CHINA:0Cr17Ni12Mo2)
305 (CHINA:1Cr18Ni12Mo2N)
316Lmod (CHINA:00Cr17Ni14Mo2N)
S21800 (Nitronic 60/218alloy)
254SMO(CHINA:00Cr20Ni18Mo6CuN)
17-4PH(630)(CHINA:0Cr17Ni4Mo4Nb)
17-7PH(631)(CHINA:0Cr17Ni7Al)
304N2 (US:UNS S30452)
AL-6XN (CHINA:00Cr20Ni24Mo7N)
Nitronic 40、UNS20904
Nitronic 50、UNS20910
Nimonic 75、UNS N06075
Nimonic 80A、UNS N07080
Nimonic 90、UNS N07090
Nimonic 263、UNS N07263
HOME ABOUT US PRODUCTS NEWS CONTACT US 中文

Stainless Steels

Nimonic 75、UNS N06075
 

Physical Properties:
Density: 8.37g/cm3                                      Melting Point:2450-2520℃
Modulus of Elasticity: 140-221GPa          Thermal Conductivity: 11.7 W/m• °C
Hardness: - Brinell 241         Electrical Resistivity( 20 - 100°C): 11.0 μm/m/°C
Approx Service Temperature:-200 to +1100°C
Main Characteristics:Good heat resistance , creep rupture resistance and mechanical properties
Applications:Used in parts of furnace, combustion chamber, gas turbine and heat-treating facility connecting piece
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Ti Fe Cu Mn Si

0.08
-
0.15

18.0
-
21.0

rem

0.20
-
0.60


0.50


0.50


1.00


1.00

 

Nimonic 80A、UNS N07080
 

Physical Properties:
Density: 8.19g/cm3                                    Melting Point:1320-1365℃
Modulus of Elasticity: 222GPa                 Thermal Conductivity:11.2 W/m• °C
Hardness: HRC32               Electrical Resistivity( 20 - 100°C):12.7 μ m/m °C
Approx Service Temperature:350 to 500°C
Main Characteristics:Precipitation hardening alloy and great promote property below 815°C
Applications:Used in bolt and vent valve at combustion chamber
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Fe Mn Si P S Al Ti Co B Zr Cu


0.10

18.0
-
21.0

rem


3.0


1.0


1.0


0.020


0.015

1.0
-
1.8

1.8
-
2.7


2.0


0.008


0.15


0.2

 

Nimonic 90、UNS N07090
 

Physical Properties:
Density: 8.18g/cm3                                   Melting Point:1310-1370 ℃
Modulus of Elasticity:227 - 240GPa      Thermal Conductivity:11.5λ / W·(m·C)-1
Hardness:-Brinell360            Electrical Resistivity( 20 - 100°C):12.7α/(10-6/℃)
Approx Service Temperature: 350°C to 550°C
Main Characteristics:Precipitation hardening alloy, Extreme high elevated temperature strength and wear strength, good elasticity
Applications:Applied in anvil manufacture, gas turbine blade and turntable
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Mn Fe Si Zr S Cu Co B Al Ti


0.13

18.0
-
21.0

rem


1.0


1.50


1.0


0.15


0.015


0.20

15.0
-
21.0


0.2

1.0
-
2.0

2.0
-
3.0

 

Nimonic 263、UNS N07263
 

Physical Properties:
Density: 8.36g/cm3                                Melting Point:1300 ℃
Modulus of Elasticity: 142-224GPa    Thermal Conductivity:11.72λ / W·(m·C)-1
Hardness:-Brinell360               Electrical Resistivity( 20 - 100°C):10.2a10-6K-1
Approx Service Temperature: 350°C to 550°C
Main Characteristics:Precipitation hardening alloy with high strength, good shaping property and ductibility in welding application
Applications:Plane-engines and components in gas turbine
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Si Ni Mo Fe Al Mn Ag B S Co Cu Ti Pb Bi

0.04
-
0.08


0.4

rem

5.6
-
6.1


0.7


0.6


0.6


0.0005


0.005


0.007

19.0
-
21.0

0.20
1.9
-
2.8

0.002


0.0001

 

 Copyright © Nanjing Interan Super Alloy CO.,LTD
 Contact: 任卫平   张利利   David
 TEL: 86-025-84170556/84190181/84170331 FAX: 86-025-84170556
 Cellphone Number: 13805152311 / 13770667940
 Zip Code: 211135
 Add:Jiannan Industry Park Cangbomen Jiangning District Nanjing CHINA
 E-mail:Inconel718@163.com / superalloycn@gmail.com
 Web: http://www.superalloy.net.cn

Internet Content Provider Licence of Ministry of Telecom&information Industry PRC Serial No.Jiangsu 0603728