Corrosion Resistant Alloy
Hastelloy B (CHINA:NS321)
Hastelloy B-2 (CHINA:NS322)
Hastelloy B-3 (CHINA: )
Hastelloy C (CHINA:NS333)
Hastelloy C-4 (CHINA: )
Hastelloy C-22 (CHINA:)
Hastelloy C-276 (CHINA:NS334)
Hastelloy C-2000 (CHINA:)
Hastelloy X (CHINA:GH3536)
Incoloy 800 (CHINA:NS111)
Incoloy 800H (CHINA:NS112)
Incoloy 825 (CHINA:NS142)
Inconel 600 (CHINA:NS312)
Inconel 625 (CHINA:NS336)
Inconel 718 (CHINA:GH4169)
UNS N04400、Monel 400
UNS N05500、Monel K500
Alloy 20 (CHINA:NS143)
Inconel 601 (CHINA:NS313)
Inconel 690 (CHINA:NS315)
Superalloys
GH1035 (RUSSIA:XH38BT)
GH2132 (US: UNSS66286)
GH3536 (US: Hastelloy X)
GH145 (US: Inconel X-750)
K406 (US: GMR-235D)
K418 (US: INCO713C)
K213 (US:ЭИ787Л)
K417 (US:IN100)
Stainless Steels
904L(CHINA:00Cr20Ni25Mo4.5Cu)
SAF 2205CHINA:00Cr22Ni5Mo3N)
SAF 2207CHINA:00Cr25Ni7Mo4N)
2RE69 (CHINA:00Cr25Ni22M02N)
Alloy 253MA (GERMANY:1.4835)
430 (CHINA:1Cr17Ni2)
310S(CHINA:0Cr25Ni20)
AISI616 (CHINA:2Cr12NiMoWV)
304(CHINA:0Cr18Ni9)
316(CHINA:0Cr17Ni12Mo2)
305 (CHINA:1Cr18Ni12Mo2N)
316Lmod (CHINA:00Cr17Ni14Mo2N)
S21800 (Nitronic 60/218alloy)
254SMO(CHINA:00Cr20Ni18Mo6CuN)
17-4PH(630)(CHINA:0Cr17Ni4Mo4Nb)
17-7PH(631)(CHINA:0Cr17Ni7Al)
304N2 (US:UNS S30452)
AL-6XN (CHINA:00Cr20Ni24Mo7N)
Nitronic 40、UNS20904
Nitronic 50、UNS20910
Nimonic 75、UNS N06075
Nimonic 80A、UNS N07080
Nimonic 90、UNS N07090
Nimonic 263、UNS N07263
 
HOME ABOUT US PRODUCTS NEWS CONTACT US 中文

Superalloys

K406 (US: GMR-235D)
 

Physical Properties:
Density: 8.05g/cm3                                    Melting Point: 1260-1345℃
Modulus of Elasticity: 145-203 GPa       Thermal Conductivity:13.82λ/(W(m•℃)
Hardness: HRC35-38           Electrical Resistivity( 20 - 100°C): 11.82a10-6-1
Main Characteristics:Has good heat-resistant high-temperature oxidation and corrosion, with good performance and the casting process of welding technology.
Applications:Below 850 ℃ the production of long-term following the work of the gas turbine blades and rotor blades and other high-temperature-oriented parts.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Mo Al Ti Fe B Zr Mn Si Sb Bi Sn P S

0.10
-
0.20

14.0
-
17.0

rem

4.5
-
6.0

3.25
-
4.0

2.0
-
3.0


1.0

0.05
-
0.10

0.03
-
0.08

0.10

0.3

0.001

0.0005

0.002

0.02


0.01

 

K418 (US: INCO713C)
 

Physical Properties:
Density: 8.0g/cm3                                      Melting Point:1295-1345℃
Modulus of Elasticity:144-211GPa         Thermal Conductivity:10.15λ/(W(m•℃)
Hardness:HRC33-37            Electrical Resistivity( 20 - 100°C):12.60a10-6-1
Main Characteristics:In the following 900 ° C has a good creep resistance, fatigue properties and antioxidant properties.
Applications:Used the 900 ° C following the work of the gas turbine rotor blades of the turbine, orientation and the entire cast turbine blades and other high-temperature parts.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Mo Al Ti Fe Nb B Zr Mn Si P S Bi
0.08
-
0.16
11.5
-
13.5
rem 3.80
-
4.80
5.50
-
6.40
0.50
-
1.00

1.0
1.80
-
2.50
0.008
-
0.020
0.06
-
0.15

0.5

0.50

0.015

0.01

0.001

 

K213 (US:ЭИ787Л)
 

Physical Properties:
Density:8.14g/cm3                                    Melting Point:1324-1361℃
Modulus of Elasticity:125-178GPa        Thermal Conductivity:10.89λ/(W(m•℃)
Hardness:HBS325                Electrical Resistivity( 20 - 100°C):12.36a10-6-1
Main Characteristics:The casting process with good performance, following the 750 ° C has a good overall performance and organizational stability.
Applications:750 ° C for the following long-term use of the runoff-pressure turbine, Axial-pressure turbine blades, gas turbines and flue gas round of mobile and static leaves.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni W Al Ti Fe B Mn P S Mo


0.10

14.0
-
16.0

34.0
-
38.0

4.0
-
7.0

1.5
-
2.0

3.0
-
4.0

rem

0.05
-
0.10


0.50


0.015


0.015


0.5

 

K417 (US:IN100)
 

Physical Properties:
Density: 7.8g/cm3                                    Melting Point: 1260-1340℃
Modulus of Elasticity:155-220GPa       Thermal Conductivity:13.2λ/(W(m•℃)
Hardness:HRC30-44                Electrical Resistivity( 20 - 100°C):13.2x10-6K-1
Main Characteristics:Is a low-density, high-intensity nickel-based superalloys casting.
Applications:Widely used in various aero-engine, turbo-rotor impeller, gunpowder starter as a whole, such as turbine
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Co Mo Al Ti Fe V B Zr Mn Si Pb S P

0.13
-
0.22

8.5
-
9.5

rem

14.0
-
16.0

2.5
-
3.5

4.8
-
5.7

4.5
-
5.0


1.0

0.6
-
0.9

0.012
-
0.022
0.05
-
0.09

0.5

0.5

0.000

0.01


0.015