Miss Zhang
 International Dept David Zhu
 
PRODUCTS
Corrosion Resistant Alloy
Hastelloy B (CHINA:NS321)
Hastelloy B-2 (CHINA:NS322)
Hastelloy B-3 (CHINA: )
Hastelloy C (CHINA:NS333)
Hastelloy C-4 (CHINA: )
Hastelloy C-22 (CHINA:)
Hastelloy C-276 (CHINA:NS334)
Hastelloy C-2000 (CHINA:)
Hastelloy X (CHINA:GH3536)
Incoloy 800 (CHINA:NS111)
Incoloy 800H (CHINA:NS112)
Incoloy 825 (CHINA:NS142)
Inconel 600 (CHINA:NS312)
Inconel 625 (CHINA:NS336)
Inconel 718 (CHINA:GH4169)
UNS N04400、Monel 400
UNS N05500、Monel K500
Alloy 20 (CHINA:NS143)
Inconel 601 (CHINA:NS313)
Inconel 690 (CHINA:NS315)
Superalloys
GH1035 (RUSSIA:XH38BT)
GH2132 (US: UNSS66286)
GH3536 (US: Hastelloy X)
GH145 (US: Inconel X-750)
K406 (US: GMR-235D)
K418 (US: INCO713C)
K213 (US:ЭИ787Л)
K417 (US:IN100)
Stainless Steels
904L(CHINA:00Cr20Ni25Mo4.5Cu)
SAF 2205CHINA:00Cr22Ni5Mo3N)
SAF 2207CHINA:00Cr25Ni7Mo4N)
2RE69 (CHINA:00Cr25Ni22M02N)
Alloy 253MA (GERMANY:1.4835)
430 (CHINA:1Cr17Ni2)
310S(CHINA:0Cr25Ni20)
AISI616 (CHINA:2Cr12NiMoWV)
304(CHINA:0Cr18Ni9)
316(CHINA:0Cr17Ni12Mo2)
305 (CHINA:1Cr18Ni12Mo2N)
316Lmod (CHINA:00Cr17Ni14Mo2N)
S21800 (Nitronic 60/218alloy)
254SMO(CHINA:00Cr20Ni18Mo6CuN)
17-4PH(630)(CHINA:0Cr17Ni4Mo4Nb)
17-7PH(631)(CHINA:0Cr17Ni7Al)
304N2 (US:UNS S30452)
AL-6XN (CHINA:00Cr20Ni24Mo7N)
Nitronic 40、UNS20904
Nitronic 50、UNS20910
Nimonic 75、UNS N06075
Nimonic 80A、UNS N07080
Nimonic 90、UNS N07090
Nimonic 263、UNS N07263
HOME ABOUT US PRODUCTS NEWS CONTACT US 中文

Corrosion Resistant Alloys

Hastelloy C-4(CHINA:NS335)
 

Physical Properties:
Density: 8.64g/cm3                                     Melting Point: 1399 °C
Modulus of Elasticity: 212.4 kN/mm2      Thermal Conductivity:10.1w/m-k
Hardness:HRC90                    Electrical Resistivity( 20 - 100°C): 12.6 μ m/m °C
Approx Service Temperature: -200 to +400°C
Main Characteristics:Stable structure property and direct usage after welding.
Applications:Apparatuses and equipments in moist chloride、hypochloric acid, hydrochloric acid and chloride atmosphere.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni Ti Fe Co Mn Si P S Mo


0.015

14.0
-
18.0

rem


7.0


3.0


2.0


1.0


0.08


0.04


0.03

14
-
17

 

Hastelloy C-22(CHINA:)
 

Physical Properties:
Density: 8.69g/cm3                                    Melting Point: 1357-1399 °C
Modulus of Elasticity: 205.5N/mm2        Thermal Conductivity:11.1 W/m-K
Hardness:HRC93                  Electrical Resistivity( 20 - 100°C): 112.6 μ m/m °C
Approx Service Temperature: -200 to+400°C
Main Characteristics:Good pitting corrosion resistance, crevice corrosion resistance and stress corrosion cracking resistance.
Applications:Sulfur dioxide cooling tower, gas cleaning system, sulfonated system ,tubular heat exchanger.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni V Fe Co Mn Si P S Mo W

0.001

20.0
-
22.5

rem


0.35

2.0
-
6.0


2.5


0.50


0.08


0.025


0.01

12.5
-
14.5

2.5
-
3.5

 

Hastelloy C-276(CHINA:NS334)
 

Physical Properties:
Density: 8.89g/cm3                                         Melting Point: 1323-1371 °C
Modulus of Elasticity: 205.5kN/mm2           Thermal Conductivity:11.1 W/m-K
Hardness:HRC90                    Electrical Resistivity( 24-100°C): 11.2 μ m/m °C
Approx Service Temperature: -200 to +400°C
Main Characteristics:Welded structure in atmosphere of strong corrosion, oxidation, reduction or warm sea water situation.
Applications:Applied in aviation, chemical industry and decarbolization in power station.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni V Fe Co Mn Si P S Mo W


0.02

14.5
-
16.5

rem


0.35

4.0
-
7.0


2.5


1.0


0.08


0.04


0.03

15
-
17

3.0
-
4.5

 

Hastelloy C-2000(CHINA:)
 

Physical Properties:
Density: 8.5g/cm3                                       Melting Point: 1399 °C
Modulus of Elasticity: 206kN/mm2          Thermal Conductivity:10.8 W / m - k
Hardness:HRC90                  Electrical Resistivity( 25 - 100°C):12.4 μ m/m °C
Approx Service Temperature: -200 to +400°C
Main Characteristics:Good corrosion resistancjiae to sulfuric acid, hydrochloric acid, hydrofluoric acid, phosphoric acid, organic acid, chloride, alkalis, pitting corrosion, crevice corrosion and stress corrosion cracking e.
Applications:Utilized in reactors , heat exchangers, valves, pumps, etc.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production

Chemical Compositions:

Chemical Compositions(%)

C Cr Ni V Fe Cu Mn Si P S Mo

0.01
23

rem


0.35

3

1.6


0.5


0.08


0.02


0.08

16

 

 Copyright © Nanjing Interan Super Alloy CO.,LTD
 Contact: 任卫平   张利利   David
 TEL: 86-025-84170556/84190181/84170331 FAX: 86-025-84170556
 Cellphone Number: 13805152311 / 13770667940
 Zip Code: 211135
 Add:Jiannan Industry Park Cangbomen Jiangning District Nanjing CHINA
 E-mail:Inconel718@163.com / superalloycn@gmail.com
 Web: http://www.superalloy.net.cn

Internet Content Provider Licence of Ministry of Telecom&information Industry PRC Serial No.Jiangsu 0603728